Durability indicators of OPC concretes subject to wick action

dc.contributor.authorDias, WPS
dc.date.accessioned2023-02-03T09:32:15Z
dc.date.available2023-02-03T09:32:15Z
dc.date.issued1993
dc.description.abstractDurability indicators for six OPC concrete mixes were obtained from wick action testing on concrete cylinders placed in water and a sodium chloride solution of concentration similar to sea water. Although 49 weeks of exposure to wick action in the salt solution was not sufficient to cause appreciable deterioration in the concretes, indirect durability indicators such as moisture transport phenomena and chloride ingress measurements were used to distinguish between the different concrete mixes. Increases in the water:cement ratio from 0·4, through 0·6, to 0·8 caused significant reductions in durability properties. An increase in cement content from 400 to 600 kg/m3 also impaired durability. However, the inclusion of 0·6% (by volume) chopped coir fibre to the control mix (w/c = 0·4, cement content = 400kg/m3) reduced durability only marginally. On the other hand, the inclusion of ultrafine gneissic quarry dust as a partial fine aggregate replacement in the control mix improved the durability indicators somewhat.en_US
dc.identifier.citationDias, W. P. S. (1993). Durability indicators of OPC concretes subject to wick action. Magazine of Concrete Research, 45(165), 263–274. https://doi.org/10.1680/macr.1993.45.165.263en_US
dc.identifier.databaseICE Virtual Libraryen_US
dc.identifier.doihttps://doi.org/10.1680/macr.1993.45.165.263en_US
dc.identifier.issn0024-9831en_US
dc.identifier.issue165en_US
dc.identifier.journalMagazine of Concrete Researchen_US
dc.identifier.pgnos263-274en_US
dc.identifier.urihttp://dl.lib.uom.lk/handle/123/20369
dc.identifier.volume45en_US
dc.identifier.year1993en_US
dc.language.isoen_USen_US
dc.publisherInstitution of Civil Engineersen_US
dc.subjectconcreteen_US
dc.titleDurability indicators of OPC concretes subject to wick actionen_US
dc.typeArticle-Full-texten_US